Equipment:
TG-DTA8122 HUM
Sample weight: 15.230 mg
Ramping rate: 10 K/min, from RT to 1273 K
Condition: 25ºC(dry) → 25ºC(90%RH), 60 min → 25ºC(dry), 240 min → Ramping start
Pan: Pt-made open
Equipment:
TG-DTA8122 HUM
Sample weight: 15.120 mg
Ramping rate: 10 K/min, from RT to 1273 K
Condition: 25ºC(dry) → 25ºC(50%RH), 60 min → 25ºC(dry), 240 min → Ramping start
Pan: Pt-made open